公司基本資料信息
|
日本原裝進(jìn)口NS銑刀MSBL230
無(wú)限涂層 長(zhǎng)柄型球頭銑刀
采用無(wú)限涂層的長(zhǎng)柄型球頭銑刀
尺寸為R0.1~R5
可進(jìn)行充分發(fā)揮長(zhǎng)柄優(yōu)勢(shì)的加工
08-00510-00010
08-00510-00015
08-00510-00020
08-00510-00025
08-00510-00030
08-00510-00035
08-00510-00040
08-00510-00045
08-00510-00050
08-00510-00055
08-00510-00060
08-00510-00065
08-00510-00070
08-00510-00075
08-00510-00080
08-00510-00085
08-00510-00090
08-00510-00095
08-00510-00100
08-00510-00110
08-00510-00120
08-00510-00125
08-00510-00130
08-00510-00140
08-00510-00150
08-00510-00160
08-00510-00170
08-00510-00180
08-00510-00190
08-00510-00200
08-00510-00210
08-00510-00220
08-00510-00230
08-00510-00240
08-00510-00250
08-00510-00260
08-00510-00270
08-00510-00280
08-00510-00290
08-00510-00300
08-00510-00400
08-00510-00500
深圳銀和國(guó)際貿(mào)易有限公司NS銑刀無(wú)限涂層 短柄型球頭銑刀(熱裝刀柄用)MSB230SF
it fits for Shrink Chuck System
買(mǎi)NS銑刀就找深圳銀和國(guó)際,保證質(zhì)量,保證品質(zhì)
短柄型(適用于熱裝式刀柄)的球頭銑刀
08-00504-00010
08-00504-00020
08-00504-00030
08-00504-00040
08-00504-00050
08-00504-00060
08-00504-00075
08-00504-00100
08-00504-00150
08-00504-00200
08-00504-00250
08-00504-00300
08-00504-00400
08-00504-00500
08-00504-00600
6切削時(shí)的傾倒:原因:進(jìn)給速度太快。切深量太多。有效長(zhǎng)度超出需要,伸出量太長(zhǎng)。使用強(qiáng)螺旋角的刀具。 對(duì)策:降低進(jìn)給速度。降低切深量。調(diào)整為最短的有效長(zhǎng)度,伸出量。使用弱螺旋角刀具
7精加工面的毛刺:原因:切削刀刃磨耗過(guò)大。使用弱螺旋角刀具。切深量太多 對(duì)策:使用新的刀具或再研磨。使用強(qiáng)螺旋角刀具。降低切深量。
8精加工表面粗糙度不良:原因:切削刀刃磨耗過(guò)大??ㄈ肭邢鳌_M(jìn)給速度太快。有效長(zhǎng)度超出需要,伸出量太長(zhǎng)。轉(zhuǎn)速太慢。中加工后的余量不均一。刀具偏擺精度不足 對(duì)策:使用新的刀具或再研磨。使用冷卻液,將切屑從切削位置中除去。降低進(jìn)給速度。調(diào)整為最短的有效長(zhǎng)度,伸出量。調(diào)高轉(zhuǎn)速。確認(rèn)中加工后的余量是否均一。調(diào)整刀具偏擺精度。
9加工精度不良:原因:主軸的伸縮量部穩(wěn)定。中加工后的余量不均一。進(jìn)給速度太快。刀具偏擺精度不足。 對(duì)策:已使用的轉(zhuǎn)速進(jìn)行暖機(jī),主軸伸縮量穩(wěn)定后再進(jìn)行加工。確認(rèn)中加工后的余量是否均一。降低進(jìn)給速度。調(diào)整刀具偏擺精度。